Development and Characterization of Novel Fore Safe Epoxy Resins

Zbigniew K. Brzozowski, Sylwia Staszczak, Pawel Koziol, Wojciech Zatorski and Dariusz Bogdal
DOI: 
https://doi.org/10.23939/chcht03.04.269
AttachmentSize
PDF icon full_text.pdf179.76 KB
Abstract: 
The curing system for newly developed solid state fire safe epoxy resins using dicyandiamide (DICY) was introduced. Composites of epoxy resins obtained from diglycidyl ether of 1,1-dichloro-2,2bis(4-hydroxyphenyl)ethylene bisphenol-C (BPC) and bisphenol-A (BPA) epoxy resins in the reaction with BPC and BPA and DICY hardener were studied. Solid epoxy resins were synthesised by the use of two different heating methods: conventional and microwave reactor. The quantities of DICY additions were 0.5–5.0 %, optimum was found to be 3 %. Limited oxygen index (OI) tests for different epoxy resins and addition of flame – retardants were carried out. The highest value of OI was 34.6. As additional flame-retardants were used zinc stannates (ZS, ZHS). Evident OI increase was noted from 27.0 for classical epoxies, 34.6 for BPC cured epoxies and 44 for cured composites with the addition of Zn/Sn flame-retardants.
References: 

[1] Lyon R.: Ultra fire-resistant thermoset polymers. Fire Research Program, Federal Aviation Administration, Technical Center Atlantic City International Airport, NJ 08405, 2005.

[2] Brzozowski Z.: Polimery, 1986, 31, 99.
https://doi.org/10.14314/polimery.1986.099

[3] Brzozowski Z.: Assistant professor theses, Warsaw University of Technology, 1986.

[4] Brzozowski Z. and Porejko S.: Polish pat. 47 344, Publ. Dec. 15, 1964.

[5] Brzozowski Z. and Porejko S.: Pat. UK 1 051 335, Publ. July 26, 1963.

[6] Factor A. and Orlando C.: J. Polym. Sci. Chem., 1980, 18, 579.
https://doi.org/10.1002/pol.1980.170180218

[7] Rusanov A.: Progress in Polym. Sci., 1994, 19, 589.
https://doi.org/10.1016/0079-6700(94)90029-9

[8] Lyon R., Castelli L. and Walters R.: Proc. BCC Conf., Stamford, Ct, USA, May 21-23, 2001, 102.

[9] Zhang P. Westmoreland R., Farris R. et al.: Polymers, 2002, 43, 5463.
https://doi.org/10.1016/S0032-3861(02)00427-5

[10] Lyon R.: Fire Resistance Mat.: Research Overview, 2000, DOT/FAA/AR/00/42.

[11] Brzozowski Z., Staszczak S., Rupinski S. et al.: J. Appl. Polym. Sci., 2006, 100, 3850.
https://doi.org/10.1002/app.21904

[12] Brzozowski Z., Staszczak S., Hadam L. et al.: Polimery, 2007, 52, 29.
https://doi.org/10.14314/polimery.2007.029

[13] Ellis B. (ed): Chemistry and technology of epoxy resins: Chapman&Hall, London 1994.
https://doi.org/10.1007/978-94-011-2932-9

[14] Brzozowski Z., Kielkiewicz J., Rawski T. et al.: Polish pat. 86401, Publ. Nov. 15, 1976.

[15] Bogdal D.: ScD-habilitation, Krakow University of Technology, Krakow 1999.

[16] Forsyth A. and Whittaker K.: J. Appl. Polym. Sci., 1999, 74, 2917.
https://doi.org/10.1002/(SICI)1097-4628(19991213)74:12<2917::AID-APP17>3.0.CO;2-U

[17] Fu B. and Hawley M.: Polym. Eng. Sci., 2000, 40, 2133.
https://doi.org/10.1002/pen.11346

[18] Cusack P., Monk A., Pearce J. and Reynolds S.: Fire and Materials, 2005, 14, 23.
https://doi.org/10.1002/fam.810140105

[19] Cusack P., Heer M. and Monk A.: Polym. Degrad. Stab., 1997, 58, 229.
https://doi.org/10.1016/S0141-3910(97)00055-4

[20] Grassie N., Johnston A. and Scotney A.: Eur. Polym. J., 1981, 17, 589.
https://doi.org/10.1016/0014-3057(81)90096-3

[21] Shen K. and Spraque R.: Plastics Compounding, 1982, 5, 67.

[22] Kicko-Walczak E.: DSc. thesis, Warsaw University of Technology, 2003.

[23] Costa L., Luda M. and Trossarelli L: Polym. Degrad. Stab., 2000, 68, 67.
https://doi.org/10.1016/S0141-3910(99)00166-4