The Study of the Mineralogical Composition and Flotation Parameters of Quartz-Graphitized Schist
Affiliation:
1Tashkent Chemical Technological Institute
32 Navoi St., 100011 Tashkent, Uzbekistan; babax2013@yahoo.com, aripova1957@yandex.ru
2Research Institute of Mineral Resources
11a Taras Shevchenko St., 100060 Tashkent, Uzbekistan; gpniimr@mail.ru
DOI:
https://doi.org/10.23939/chcht10.03.343
Attachment | Size |
---|---|
full_text.pdf | 247.77 KB |
Abstract:
Exploration studies in Uzbekistan revealed one graphite deposit (Taskazgan) and about 25 sites with varying perspective degree. In order to obtain the graphite for refractory industry uses insufficiently known Rupat, Zauchak and Zahchahona sites were studied. According to the research, Zahchahona site can be classified as a medium-sized field; the refined graphite content in the ore deposit is 3 to 15 %, which meets the requirements of the industry for this type of raw material. Graphite was refined by flotation and leaching process, brought to grade of 75 % carbon.
References:
[1] ASTM Designation: C 561-91, Standart Test Method for Ash in Graphite Sample.
[2] ASTM Designation: C 562-91, Standart Test Method for Mousture in Graphite Sample.
[3] Khamidov R.: Geologia i Mineral. Res., 2011, 2, 34.
[4] http://ww.total.net/~bogdan/graphite.html.
[5] Babakhanova Z. and Aripova M.: Khim. Prom., 2015, 1, 12.
[6] Bezuglov E.: Report on the Results of the GSP Surhantauskoy Geological Survey Scale of 1: 50,000 in the 1966-68 Biennium, Funds of Goscomgeology of Uzbekistan. Tashkent 1969, 352.
[7] Walker P., Rakszawski J. and Amington A.: ASTM Bulletin, 1955, 208, 52.