Photodegradation of Pharmaceuticals Studied with UV Irradiation and Differential Scanning Calorimetry

Kevin Menard1, Witold Brostow2 and Noah Menard2
Affiliation: 
1 PerkinElmer LSAS, 761 Bridgeport Ave, MS71, Shelton, CT 06484, USA; kevin.menard@perkinelmer.com 2 Laboratory of Advanced Polymers & Optimized Materials (LAPOM), Department of Materials Science and Engineering, University of North Texas, 3940 Nort Elm Street E-132, Denton, TX 76207, USA; http://www.unt.edu/LAPOM/;wbrostow@yahoo.com, nrcmenard@gmail.com
DOI: 
https://doi.org/10.23939/chcht05.04.385
AttachmentSize
PDF icon full_text.pdf177.51 KB
Abstract: 
Given rapidly increasing concerns about photodegradation of pharmaceuticals, we have applied accurate methods to quantitatively evaluate the drug photostability. The drugs studied were nifedrine, acetylsalicylic acid, acetaminophen, cetirizine, and pantoprazole. UV energy striking a target has been determined by using graphite. Runs were performed by placing each sample in a pan with a quartz lid and exposing it to ultraviolet (UV) light for periods of time ranging from 1 to 120 seconds. Percentage decomposition as a function of time has been determined for each pharmaceutical. Fast differential scanning calorimetry (DSC) in situ was used to evaluate changes in thermophysical behavior of the drugs and possible formation of new phases. The UV degradation rates so determined cover a very wide range, from 0.1 to 20.0 %/s. Factors affecting the photodegradability are discussed.
References: 

[1] Tonneson H.: Photostability of Drugs and Drug Formulations. Taylor and Francis, Boca Raton, FL 2006.

[2] U.S. Pharmacopedia, Impurities Track, 26 September 2006, Retrieved on February 26, 2009, from http://www.usp.org/pdf/EN/eventsEducation/asMeeting/2006Denver/presentat...

[3] Albini A.: Drugs Photochemistry and Photostability. Royal Society of Chemistry, London 1998.

[4] ICH Q1B, Photostability Testing of New Drug Substances and Products, IFPMA, Geneva 1996.

[5] ICH Q1A, Stability Testing of New Drug Substances and Products, IFPMA, Geneva 1992.

[6] Garfield E.: J. Mater. Ed., 1994, 16, 327.
https://doi.org/10.1111/j.1467-9639.1994.tb00691.x

[7] Menard K.: Thermal transitions and their measurement, Ch. 8 [in:] Brostow W. (Ed.), Performance of Plastics. Hanser, Munich - Cincinnati 2000.

[8] Lucas E., Soares B. and Monteiro E.: Caracterização de polimeros, e- papers, Rio de Janeiro 2001.

[9] Gedde U.: Polymer Physics. Springer-Kluver, Dordrecht-Boston 2001.

[10] Saiter J.-M., Negahban M., dos Santos Claro P. and Garda M.-R.: J. Mater. Ed., 2008, 30, 51.
https://doi.org/10.17771/PUCRio.PDPe.12037

[11] Brostow W., Chiu R., Kalogeras I. and Vassilikou-Dova A.: Mater. Lett., 2008, 62, 3152.
https://doi.org/10.1016/j.matlet.2008.02.008

[12] Kalogeras I. and Brostow W.: J. Polymer Sci. Phys., 2009, 47, 80.
https://doi.org/10.1002/polb.21616

[13] Babu R., Brostow W., Kalogeras I. and Sathigari S.: Mater. Lett., 2009, 63, 2666.
https://doi.org/10.1016/j.matlet.2009.09.033

[14] Fouassier J.: Photoinitiation, Photopolymerization and Photocuring. Hanser-Gardner, Munich-Cincinnati 1995.

[15] Tonneson H.: Formulation Approaches for Improving Solubility and Impact on Drug Photostability, Ch. 16 [in:] TonnesonH.: Photostability of Drugs and Drug Formulations. Taylor and Francis, Boca Raton, FL 2006.

[16] Albini A. and Fasani E.: Rationalizing the Photochemistry of Drugs, Ch. 4 [in:] TonnesonH.: Photostability of Drugs and Drug Formulations. Taylor and Francis, Boca Raton, FL 2006.